Reading the AISI 316 Burnishing Comparison for Bore Applications
What an external-surface AISI 316 experiment establishes, and what an internal-bore trial must still measure.
What an external-surface AISI 316 experiment establishes, and what an internal-bore trial must still measure.
Read the tested chip-mouth changes, minimum-flow comparison and transfer limits for a 30 mm ejector head in 42CrMo4+QT.