Independent industry mediaMethods / Tooling / Bore qualityFollow the publication

Novel BTA Tools for Nickel Superalloys: Boring and Solid Drilling Scope

Identify the 2025 novel BTA boring-tool paper, distinguish its publication scope from solid drilling and preserve the evidence needed to interpret an …

Deep Hole Drilling Superalloys: A Complete Inconel 718 Cooling Experiment

Read the implemented CO2/lubricant architecture of an Inconel 718 experiment, distinguish pressure from mass flow and retain its tool-life endpoint.